9. Broken horn
Reason:
The incoming edge of the battery sheet is missing.
Preventive measures:
The incoming materials should be screened strictly, and the broken corners should be detected and returned to the manufacturer.

10. Broken porcelain
Reason:
The incoming edge of the battery is poorly coated.

Preventive measures:
The incoming materials are strictly screened, and the broken porcelain is detected and returned to the manufacturer.

11, Welding tape offset (exposed)
Reason:
A. During welding, the positioning of the interconnection bar deviates from the position of the welding printing line on the battery.
B. The temperature is too high, and the hardness of the welding belt is too high, causing the battery sheet to bend after welding.
C. When working, the interconnection bar is spot-welded and distorted, resulting in deviation.

Preventive measures:
a. The placement of the battery on the upper side of the baseplate will cause the welding tape deviation.
b. The main grid line deviation of the raw material of the battery will cause the welding strip to offset the main grid line after welding.
c. The interconnected strip with deformed welding tape cannot be used.

12, Virtual welding, over welding
Reason:
A. The welding temperature is too low, and the temperature of the low plate is too low.
B. Too little flux.
C. Too fast a speed will cause virtual welding.
D. Too high welding temperature or too long welding time will lead to over-welding phenomenon.

Preventive measures:
a. Ensure that the welding temperature parameters are set. And to check regularly, welding time is 3-4 seconds.
b. To ensure the temperature of the soldering iron, welding time and the use of flux when repairing.
c. Strengthen EL inspection to avoid bad leakage in the next process.
d. Regularly manage the soaking solution and time of the interconnection bar.